{"product_id":"cedcaeittmmoa","title":"IrO2-Ta2O5-TiO2 Mixed Metal Oxide (MMO) as Dimensionally Stable Anode (DSA) for Electrodialysis, Chlorine-Alkali Electrolysis, and Wastewater Treatment, CEDCAEITTMMOA","description":"\u003cp\u003eAn Iridium-Tantalum-Titanium (Ir-Ta-Ti) Mixed Metal Oxide (MMO) Anode is an advanced insoluble electrode engineered specifically for oxygen evolution reactions (OER) and aggressive acidic environments.\u003c\/p\u003e\n\u003cp\u003eThe composition of Iridium-Tantalum-Titanium (Ir-Ta-Ti) Mixed Metal Oxide (MMO) anode is: (1) \u003cstrong\u003eTitanium Substrate (Grade 1\/2)\u003c\/strong\u003e: It uses high-purity titanium mesh, plate, or tubular forms to provide structural strength and act as the core current collector. (2) \u003cstrong\u003eIrO2 -Ta2O5 Active Coating\u003c\/strong\u003e: Iridium dioxide delivers exceptional electrocatalytic activity for oxygen generation. Tantalum pentoxide acts as a stable, inert binder that prevents substrate passivation and coating delamination.\u003c\/p\u003e\n\u003cp\u003eThe main electrochemical advantages are: (1) \u003cstrong\u003eLow Oxygen Overpotential\u003c\/strong\u003e: The catalytic coating lowers the activation energy barrier for water splitting, reducing cell voltage and saving energy during continuous operation. (2) \u003cstrong\u003eExceptional Acid Resistance\u003c\/strong\u003e: It remains chemically stable in strong acid electrolytes (such as sulfuric or nitric acid), resisting rapid dissolution or peeling. (3) \u003cstrong\u003eDimensional Stability\u003c\/strong\u003e: Unlike consumable lead or graphite alternatives, it doesn't deform or erode, keeping inter-electrode spacing constant over thousands of operating hours.   \u003c\/p\u003e\n\u003ctable style=\"width: 101.819%; height: 351.05px;\" width=\"100%\"\u003e\n\u003ctbody\u003e\n\u003ctr style=\"height: 35.6px;\"\u003e\n\u003ctd style=\"width: 30.2548%; height: 35.6px;\"\u003e\u003cem\u003ePart Number\u003c\/em\u003e\u003c\/td\u003e\n\u003ctd style=\"width: 69.3567%; height: 35.6px;\"\u003e\n\u003cp\u003e\u003cspan\u003eCEDCAEITTMMOA (C-EDCAE-ITTMMOA)\u003c\/span\u003e\u003c\/p\u003e\n\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr style=\"height: 106.8px;\"\u003e\n\u003ctd style=\"width: 30.2548%; height: 106.8px;\"\u003e\u003cem\u003eTi Substrate\u003c\/em\u003e\u003c\/td\u003e\n\u003ctd style=\"width: 69.3567%; height: 106.8px;\"\u003e\n\u003cp\u003e\u003cspan\u003e(1) Ti Plate, thickness of 1 mm\u003c\/span\u003e\u003c\/p\u003e\n\u003cp\u003e\u003cspan\u003e(2) Ti Mesh, thickness of 1 mm\u003c\/span\u003e\u003c\/p\u003e\n\u003cp\u003e\u003cspan\u003eElectrode Tab is welded on the substrate\u003c\/span\u003e\u003c\/p\u003e\n\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr style=\"height: 71.2px;\"\u003e\n\u003ctd style=\"width: 30.2548%; height: 71.2px;\"\u003e\n\u003cp\u003e\u003cem\u003eActive Coating Material\u003c\/em\u003e\u003c\/p\u003e\n\u003c\/td\u003e\n\u003ctd style=\"width: 69.3567%; height: 71.2px;\"\u003e\n\u003cp\u003e\u003cspan\u003eIrO2+Ta2O5+TiO2, coating thickness of 8-15 um\u003c\/span\u003e\u003c\/p\u003e\n\u003cp\u003e\u003cspan\u003eThe loading mass of noble metal is 15-40 g\/m2\u003c\/span\u003e\u003c\/p\u003e\n\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr style=\"height: 35.6px;\"\u003e\n\u003ctd style=\"width: 30.2548%; height: 35.6px;\"\u003e\u003cem\u003eAnode Size\u003c\/em\u003e\u003c\/td\u003e\n\u003ctd style=\"width: 69.3567%; height: 35.6px;\"\u003e\n\u003cp\u003e\u003cspan\u003e50*100 mm\u003c\/span\u003e\u003c\/p\u003e\n\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr style=\"height: 35.6px;\"\u003e\n\u003ctd style=\"width: 30.2548%; height: 35.6px;\"\u003e\u003cem\u003ePotential for OER\u003c\/em\u003e\u003c\/td\u003e\n\u003ctd style=\"width: 69.3567%; height: 35.6px;\"\u003e\n\u003cp\u003e\u003cspan style=\"color: rgb(0, 0, 0);\"\u003e\u0026gt;1.45 V (suitable for H2SO4 solution system)\u003c\/span\u003e\u003c\/p\u003e\n\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr style=\"height: 22.4px;\"\u003e\n\u003ctd style=\"width: 30.2548%; height: 22.4px;\"\u003e\u003cem\u003eAcceptable Voltage \u0026amp; Current Density\u003c\/em\u003e\u003c\/td\u003e\n\u003ctd style=\"width: 69.3567%; height: 22.4px;\"\u003e\n\u003cdiv style=\"text-align: left;\"\u003e1-15 V; 1-10 A \u003c\/div\u003e\n\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003ctr style=\"height: 43.85px;\"\u003e\n\u003ctd style=\"width: 30.2548%; height: 43.85px;\"\u003e\u003cem\u003ePackage Size\u003c\/em\u003e\u003c\/td\u003e\n\u003ctd style=\"width: 69.3567%; height: 43.85px;\"\u003e1 pcs\/pack\u003c\/td\u003e\n\u003c\/tr\u003e\n\u003c\/tbody\u003e\n\u003c\/table\u003e\n\u003cp\u003e\u003cbr\u003e\u003c\/p\u003e\n\u003cp\u003e\u003cspan\u003e\u003cstrong\u003eNotes\u003c\/strong\u003e: Please try to store the IrO2-Ta2O5-TiO2 MMO anode in a dry place.\u003c\/span\u003e\u003c\/p\u003e\n\u003cp\u003e\u003cspan\u003e\u003cstrong\u003eReferences\u003c\/strong\u003e: \u003c\/span\u003e\u003c\/p\u003e\n\u003col\u003e\n\u003cli\u003e\u003cspan\u003e\u003ca href=\"https:\/\/www.sciencedirect.com\/science\/article\/abs\/pii\/S0013468626001258\"\u003eZ. Li, et al. Mechanistic insights into the durability of IrO2–Ta2O5 DSA influenced by organic additives in a copper electroplating system, Electrochimica Acta, 2026, 553, 148232\u003c\/a\u003e\u003c\/span\u003e\u003c\/li\u003e\n\u003cli\u003e\u003cspan\u003e\u003ca href=\"https:\/\/www.sciencedirect.com\/science\/article\/abs\/pii\/S0043135426006044\"\u003eJ. Wang, et al. Enhanced bioelectrochemical anaerobic membrane bioreactor utilizing IrO2-Ta2O5\/Ti bioanode for municipal wastewater treatment: Synchronizing organic carbon recovery and membrane fouling mitigation, Water Research, 2026, 299, 125922\u003c\/a\u003e \u003c\/span\u003e\u003c\/li\u003e\n\u003c\/ol\u003e","brand":"SETGY","offers":[{"title":"IrO2-Ta2O5-TiO2 on Ti Plate","offer_id":68050716393702,"sku":"CEDCAERITMMOATP","price":99.0,"currency_code":"USD","in_stock":true},{"title":"IrO2-Ta2O5-TiO2 on Ti Mesh","offer_id":68050716426470,"sku":"CEDCAERITMMOATM","price":99.0,"currency_code":"USD","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0774\/6591\/1526\/files\/CEDCAERITMMOA_main.jpg?v=1794816326","url":"https:\/\/echemsupplies.com\/products\/cedcaeittmmoa","provider":"EChem Supplies","version":"1.0","type":"link"}