Skip to product information
Ni0.95Co0.04Al0.01(OH)2 Precursor Powder for LNCA (or NCA) Cathode Synthesis, 100 g/bottle, CLIBPCNCA95OH

Ni0.95Co0.04Al0.01(OH)2 Precursor Powder for LNCA (or NCA) Cathode Synthesis, 100 g/bottle, CLIBPCNCA95OH

$99.00 USD
In Stock SKU: CLIBPCNCA95OH
Use your own shipping account?

We support FedEx, UPS, and DHL third-party billing for institutional customers.

Place your order first, then email shipping@echemsupplies.com with your account details and order number. We'll generate the label using your account and refund your shipping charges, less a handling fee.

Review third-party shipping terms →


The Ni0.95Co0.04Al0.01(OH)2 is obtained by co-precipitation method, which can be mixed with lithium salts (eg: LiOH) to synthesize the LNCA cathode powder. The precursor reacts with the lithium source at temperatures typically between 750-850 degrees to form the final layered oxide cathode material.

Part Number

CLIBPCNCA95OH (C-LIB-PC-NCA95OH)

Chemical Composition

Ni: 95.0 mol%,  Co: 0.04 mol%,  Al: 0.01 mol%

 Particle Size Distribution

D10 = 5.3 um;  D50 =8.1 um;   D90 = 13.6 um

Tap Density 1.98 g/cm3
Specific Area 7.21 m2/g

 

Notes: (1) Please store the NCA95OH precursor powder in a dry area (glovebox is preferred); (2) The battery powder is highly recommended to be dried at 80-100°C in a vacuum oven for 6-12 h before use. 

References

  1. U. H. Kim, et al. High-Energy W-Doped Li[Ni0.95Co0.04Al0.01]O2 Cathodes for Next-Generation Electric Vehicles, Energy Storage Mater,, 2020, 33, 399-407
  2. B. C. Lee, et al. Structural Analysis of Deeply Charged Li(Ni0.95Co0.04Al0.01)O2 Cathode for Li-Ion Battery, ChemSusChem 2025, 18, e202401856

You may also like