Skip to product information
Ni0.5Co0.2Mn0.3(OH)2 Precursor Powder for NCM523 Cathode Synthesis, 100 g/bottle, CLIBPCNCM523OH

Ni0.5Co0.2Mn0.3(OH)2 Precursor Powder for NCM523 Cathode Synthesis, 100 g/bottle, CLIBPCNCM523OH

$99.00 USD
In Stock SKU: CLIBPCNCM523OH
Use your own shipping account?

We support FedEx, UPS, and DHL third-party billing for institutional customers.

Place your order first, then email shipping@echemsupplies.com with your account details and order number. We'll generate the label using your account and refund your shipping charges, less a handling fee.

Review third-party shipping terms →


The Ni0.5Co0.2Mn0.3(OH)2 with spherical morphology is obtained by co-precipitation method, which can be mixed with lithium salts (eg: LiOH) to synthesize the NCM523 cathode powder. The precursor reacts with the lithium source at temperatures typically between 800-950 degrees to form the final layered oxide cathode material.

Part Number

CLIBPCNCM523OH (C-LIB-PC-NCM523OH)

Chemical Composition

Ni: 60.2 mol%,  Co: 9.90 mol%,  Mn: 29.9 mol%

 Particle Size Distribution

D10 = 2.3 um;  D50 =3.5 um;   D90 = 5.2 um

Tap Density 1.31 g/cm3
Specific Area 20.7 m2/g

 

Notes: (1) Please store the NCM523OH precursor powder in a dry area (glovebox is preferred); (2) The battery powder is highly recommended to be dried at 80-100°C in a vacuum oven for 6-12 h before use. 

References

  1. K. Xu, et al. Effect of precursor and synthesis temperature on the structural and electrochemical properties of Li(Ni0.5Co0.2Mn0.3)O2, Electrochimica Acta. 2012, 75, 393-398.
  2. H. Dong, et al. Single-Crystal Materials Regenerated and Modified by Spent NCM523 as a High-Voltage Stable Cycling Cathode Material, J. Solid State Electrochem., 2014, 18, 1789–1797