Ni0.9Co0.05Mn0.05(OH)2 Precursor Powder for Single-Crystal NCM9055 Cathode Synthesis, 100 g/bottle, CLIBPCSCNCM9055OH

Ni0.9Co0.05Mn0.05(OH)2 Precursor Powder for Single-Crystal NCM9055 Cathode Synthesis, 100 g/bottle, CLIBPCSCNCM9055OH

$99.00 USD
In Stock SKU: CLIBPCSCNCM9055OH
Use your own shipping account?

We support FedEx, UPS, and DHL third-party billing for institutional customers.

Place your order first, then email shipping@echemsupplies.com with your account details and order number. We'll generate the label using your account and refund your shipping charges, less a handling fee.

Review third-party shipping terms →


The Ni0.9Co0.05Mn0.05(OH)2 is obtained by co-precipitation method, which can be mixed with lithium salts (eg: Li2CO3, LiOH) to synthesize the NCM9055 cathode powder. The precursor reacts with the lithium source at temperatures typically between 750-850 degrees to form the final layered oxide cathode material.

Part Number

CLIBPCSCNCM9055OH (C-LIB-PC-SCNCM9055OH)

Chemical Composition

Ni: 90.2 mol%,  Co: 4.81 mol%,  Mn: 4.99 mol%

 Particle Size Distribution

D10 = 2.5 um;  D50 =3.6 um;   D90 = 5.1 um

Tap Density 1.94 g/cm3
Specific Area 8.64 m2/g

 

Notes: (1) Please store the NCM9055OH precursor powder in a dry area (glovebox is preferred); (2) The battery powder is highly recommended to be dried at 80-100°C in a vacuum oven for 6-12 h before use. 

References

  1. S. Zhang, et al. Structural engineering of nickel-rich cathode material for improved cycling performance of lithium-ion batteries, J. Energy Chem., 2026, 114,  52-59
  2. J. Wang, et al. Co-Precipitation of Ni-Rich Me(OH)2 Precursors for High Performance LiNixMnyCo1-x-yO2 Cathodes: A Review, Energy Environ. Mater., 2025, 8, e70078

You may also like