Ni0.95Co0.04Al0.01(OH)2 Precursor Powder for LNCA (or NCA) Cathode Synthesis, 100 g/bottle, CLIBPCNCA95OH
Use your own shipping account?
We support FedEx, UPS, and DHL third-party billing for institutional customers.
Place your order first, then email shipping@echemsupplies.com with your account details and order number. We'll generate the label using your account and refund your shipping charges, less a handling fee.
The Ni0.95Co0.04Al0.01(OH)2 is obtained by co-precipitation method, which can be mixed with lithium salts (eg: LiOH) to synthesize the LNCA cathode powder. The precursor reacts with the lithium source at temperatures typically between 750-850 degrees to form the final layered oxide cathode material.
| Part Number |
CLIBPCNCA95OH (C-LIB-PC-NCA95OH) |
| Chemical Composition |
Ni: 95.0 mol%, Co: 0.04 mol%, Al: 0.01 mol% |
| Particle Size Distribution |
D10 = 5.3 um; D50 =8.1 um; D90 = 13.6 um |
| Tap Density | 1.98 g/cm3 |
| Specific Area | 7.21 m2/g |
Notes: (1) Please store the NCA95OH precursor powder in a dry area (glovebox is preferred); (2) The battery powder is highly recommended to be dried at 80-100°C in a vacuum oven for 6-12 h before use.