Na3V2(PO4)3 (NVP) Powder for Na-Ion Battery Cathode, 50-500 g/bottle, CSIBCNVP
Use your own shipping account?
We support FedEx, UPS, and DHL third-party billing for institutional customers.
Place your order first, then email shipping@echemsupplies.com with your account details and order number. We'll generate the label using your account and refund your shipping charges, less a handling fee.
Na3V2(PO4)3 (NVP) is a highly promising, low-cost cathode material for Sodium-Ion Batteries (SIBs). It belongs to polyanion family of electrode materials and is distinguished by its stable, three-dimensional NASICON (Na super ionic conductor) structure. The reaction is sustained by the V3+/V4+ redox couple. The primary reaction typically occurs at a remarkably flat and high voltage plateau of ~3.4 V vs. (Na/Na+) and its theoretical specific capacity can be up to 117.6 mAh/g.
| Part Number |
CSIBCNVP (C-SIB-C-NVP) |
| Chemical Formula |
Na3V2(PO4)3 |
| Chemical Composition |
Na: 17.56 wt%, Fe: 20.21 wt%, C: 20.02 wt%) |
| Particle Size Distribution |
D10: 0.41 um, D50 =1.69 um, D90: 10.35 um |
| Tap Density | 0.57 g/cm3 |
| Specific Area | 20.72 m2/g |
| XRD |
![]() |
| First Discharging Capacity |
~112 mAh/g (0.2 C)
|
| First Columbic Efficiency |
96.3% |
| Package Grade |
50 g, 100 g, 200 g, and 500 g/bottle |