Skip to product information
GelMA (Gelatin Methacrylate) Powder for Photocurable Hydrogel Synthesis, 1 g/bottle, CPCHSGelMA

GelMA (Gelatin Methacrylate) Powder for Photocurable Hydrogel Synthesis, 1 g/bottle, CPCHSGelMA

$139.00 USD
In Stock SKU: CPCHSGelMADS30
Use your own shipping account?

We support FedEx, UPS, and DHL third-party billing for institutional customers.

Place your order first, then email shipping@echemsupplies.com with your account details and order number. We'll generate the label using your account and refund your shipping charges, less a handling fee.

Review third-party shipping terms →


GelMA (Gelatin Methacrylate) is one of the most widely used photocrosslinkable biopolymers for tissue engineering, 3D bioprinting, and cell encapsulation. By grafting methacrylate groups onto the amine-rich backbone of hydrolyzed collagen (gelatin), GelMA allows for rapid, cytocompatible photo-crosslinking under UV or visible light in the presence of a photoinitiator.

Part Number

CPCHSGelMA (C-PCHS-GelMA)

Chemical Formula/Structure
Degree of Substitution
(1) ~30%, compression modulus: 1-10 kPa, suitable for cell culture and drug delivery. 

(2) ~60%, compression modulus: 3.5-22 kPa, suitable for soft tissue engineering and microfluid chip

(3) ~90%, compression modulus: 5.12-48 kPa, suitable for 3D bioprinting and support bracket 
Photoinitiator
The photoinitiator LAP (0.05 g) is included. 
Hydrogel Preparation Steps

(1). 0.25% (2.5 mg/mL) photoinitiator PLA solution preparation: Take 20 mL PBS into 0.05 g LAP brown bottle and heated it at 40-50°C for 15 min. Several times of manual vibration can be applied.  

(2) 5-30% (50-300 mg/mL) GelMA solution preparation: Weigh calculated amount of GelMA powder into a centrifuge tube and add the photoinitiator PLA solution for mixing. Heat it up to 60-70 °C until full dissolution (avoid light).

(3) Gel Formation: Expose the mixing solution at 405 nm light source. The hydrogel strength can be adjusted by illumination time and light intensity.    

Storage Conditions

Store it at -20°C (18 months), and 4°C for use in 7 days after de-freeze. 

Package Size 1 g/bottle

 

References: 

  1. Y. C. Chen, et al. Functional Human Vascular Network Generated in Photocrosslinkable Gelatin Methacrylate Hydrogels, Adv. Funct. Mater., 2012, 22, 2027-2039
  2. J. Ramón-Azcón, et al. Gelatin methacrylate as a promising hydrogel for 3D microscale organization and proliferation of dielectrophoretically patterned cells, Lab Chip (2012) 12 (16): 2959–2969.

御溪生物

You may also like